Baker Hughes pioneers flexible pipe solution to overcome stress corrosion cracking

Baker Hughes has reached a significant technology milestone in pioneering a solution to overcome flexible pipe stress corrosion cracking (SCC) tendencies in high CO2 content fields, such as those found in Brazil’s pre-salt offshore developments.

View the full article